項(xiàng)目 | 聚輕高鋁磚 | |||||
0.6 | 0.7 | 0.8 | 0.9 | 1.0 | 1.2 | |
Al2O3/% | ≥48 | ≥48 | ≥48 | ≥48 | ≥48 | ≥48 |
Fe2O3/% | ≤2 | ≤2 | ≤2 | ≤2 | ≤2 | ≤2 |
體密(g/cm3) | ≤0.6 | ≤0.7 | ≤0.8 | ≤0.9 | ≤1.0 | ≤1.2 |
耐壓強(qiáng)度 Mpa | ≥2.0 | ≥2.5 | ≥2.9 | ≥3.4 | ≥3.9 | ≥5.00 |
導(dǎo)熱性(350°C)W/m.K | ≤0.30 | ≤0.35 | ≤0.35 | ≤0.45 | ≤0.50 | ≤0.55 |
再熱線性變化 2.0% °C | 1350 | 1350 | 1400 | 1400 | 1400 | 1400 |